Method for Increasing the Dewatering of a sheet of paper into a Paper making machine, which comprises Adding to the sheet of paper from 00226 to 6795 kg / ton.Based on the weight of the dry Fiber, one or more Polymers functionalized with aldehyde, whose Average Molecular weight is at least 300 g / mol.
Method for Increasing the Dewatering of a sheet of paper into a Paper making machine, which comprises Adding to the sheet of paper from 00226 to 6795 kg / ton.Based on the weight of the dry Fiber, one or more Polymers functionalized with aldehyde, whose Average Molecular weight is at least 300 g / mol.
展开▼
机译:一种增加纸张在造纸机中脱水的方法,该方法包括向纸张中添加00226至6795 kg / t。基于干纤维的重量,一种或多种经醛官能化的聚合物,其平均分子量至少为300 g / mol。
Method for Increasing the Dewatering of a sheet of paper comprising Adding to the sheet of paper from 00226 to 6795 kg / ton, based on the dry weight of the FibreOne or more Polymers functionalized with amino or aldehyde, which has groups and amido, such Polymers have a Molecular Weight of at least 100000 GS / Bad.