The present invention is a, and more particularly relates to a stone and cement-like artificial stone of the basalt by the basalt-like artificial stone manufacturing method and a second method comprising the steps of: mixing a 1; Lubricate the foam mold for containing the mixture spray the foam particles thereon step; The mixture was poured into the foam mold and is further step spray the foam particles, once on the mixture; After drying the mixture by subtracting from the step that the metal mold and; Positioning the demold the contents immersed in a liquid quick-setting admixture for 10 to 12 time steps, and; And the contents taken out from the binary-setting admixture and the clear water phase leaving soak for 24 hours; After drying of the contents taken out from the binary of water, placing immersed in gasoline or thinner and; The method comprising the steps of painting the glaze binary contents taken out from the gasoline or thinner; And a step for drying the contents of the said glazed painted, provides artificial stone of the basalt-like manufactured by the same method as described above.
展开▼