In talgyu method of the invention In the accelerator by the talgyu efficiency improved hot metal in order to adjust the ray of the input location and the time of deregulation to repair the hot metal chulseon from the blast furnace to the ray (3), and to facilitate the talgyu reaction It relates, comprising the steps of: in the 30 to 50% of the total deregulation input before the molten iron in the repair of the ray; In the step of generating natang site generated during repair the hot metal into the ray of fluorite (CaF2) in the molten iron per tonne and 0.6 ~ 1.2㎏; It provides the hot metal after the start talgyu repair method of this talgyu efficiency characterized in that from 1/5 of the total time of the molten iron repair time comprising: In the rest deregulation occurred in natang improved hot metal parts.; Thus, the present invention has the effect of suppressing the excessive developer overflows the slag caused by suppressing the foaming phenomenon occurring during operation and talgyu, whereby the ladle can it is possible to uniformly manage the dose improve silsuyul.
机译:在本发明的talgyu方法中,通过talgyu效率提高铁水的促进剂,以便调节输入位置的射线和解除管制的时间,以将高炉铁水从射线炉修复到射线(3),并促进talgyu反应涉及,包括以下步骤:在铁水修复射线之前,在总的失调输入的30%到50%之间;在修补过程中产生的纳塘部位,铁水进入铁水中的萤石射线(CaF2)射线每吨和0.6〜1.2㎏;它提供了一种在启动talgyu修复方法之后的铁水,该talgyu效率的特征在于,从总铁水修复时间的1/5开始:因此,本发明具有抑制过量的显影剂溢出的效果,所述显影剂由于抑制在操作期间发生的起泡现象和滑石而引起的炉渣溢出,从而可以将钢水包均匀地管理剂量提高的硅藻土。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号