PURPOSE: A hydroxyapatite whisker£Ca10(PO4)6(OH)2| containing Si and Mg by a hydrothermal method is provided for use as reinforcing materials of biotissue and medical substances due to improved biological affinity compared with conventional hydroxyapatite whisker. CONSTITUTION: The hydroxyapatite whisker containing Si and Mg is characterized by substituting P for Si and Ca for Mg in the hydroxyapatite£Ca10(PO4)6(OH)2| crystal structure, wherein the amounts of Si and Mg are 0.1-5wt.% and 0.1-1wt.%, respectively. The preparation method of hydroxyapatite whisker comprises the steps of: preparing hydroxyapatite powder containing Si and Mg; adding organics such as citric acid, lactic acid, ethylenediamine tetraacetic acid(EDTA), etc.; hydrothermal reacting at 200deg.C for 24hrs. in a high pressure vessel; washing and drying at 100deg.C. The resultant hydroxyapatite particles have a whisker shape and an aspect ratio over 10.
机译:用途:羟基磷灰石晶须£Ca10(PO4)6(OH)2 |与常规的羟基磷灰石晶须相比,由于具有改善的生物亲和性,因此提供了通过水热法含有Si和Mg的Si和Mg作为生物组织和药物的增强材料。组成:含有Si和Mg的羟磷灰石晶须的特征是在羟磷灰石Ca10(PO4)6(OH)2 |中用P代替Si和Ca代替Mg。晶体结构,其中Si和Mg的含量分别为0.1-5wt。%和0.1-1wt。%。羟基磷灰石晶须的制备方法包括以下步骤:制备含Si和Mg的羟基磷灰石粉末;制备含Si和Mg的羟基磷灰石粉末。加入柠檬酸,乳酸,乙二胺四乙酸(EDTA)等有机物;在200℃水热反应24小时。在高压容器中;洗涤并在100℃下干燥。所得羟基磷灰石颗粒具有晶须形状,长径比超过10。

著录项

  • 公开/公告号KR100473276B1

    专利类型

  • 公开/公告日2005-03-08

    原文格式PDF

  • 申请/专利权人

    申请/专利号KR20010076509

  • 申请日2001-12-05

  • 分类号C01B25/32;

  • 国家 KR

  • 入库时间 2022-08-21 22:04:09

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号