首页> 外国专利> METHOD FOR PRODUCING shaped door skins FROM WOOD composite door skins, manufacturing in this way, and the door made with the door skin THIS

METHOD FOR PRODUCING shaped door skins FROM WOOD composite door skins, manufacturing in this way, and the door made with the door skin THIS

机译:用木质复合门板生产异型门板的方法,以此方式制造,以及用门板制成的门

摘要

1. A process for converting a flat previously formed blank into a molded door skin molded, comprising the following steps: a) perform a solid slab of medium density fiberboard; b) moistening the blank and allowing the swelling fibers; c) placing the heated billet between plates press, the plates are heated to a temperature sufficient to soften the resin in the blank and thus to soften the blank; d) applying a pressure sufficient for clamping the plates and tog To thereby deform the preform into a shaped form defined by the configuration of plates; e) degassing the blank; and f) removing the molded blank from the contoured space between plitami.2. A method according to claim 1, comprising the step of: a) applying pressure to the plates, at least during the three tsiklov.3. A method according to claim 2, comprising the step of: a) applying pressure to the plates is not more than six tsiklov.4. A method according to claim 2, comprising the step of: a) applying a pressure in the first cycle to the first predetermined level over a period of time greater than the time period during which pressure is applied in any subsequent tsikle.5. A method according to claim 2, comprising the step of: a) maintaining the pressure in the last cycle for a period exceeding the period of time during which the pressure is maintained in the first tsikle.6. A method according to claim 1, comprising a workpiece degassing operation by removing moisture through apertures in at least one of plit.7. A method according to claim 6, comprising the step of: a) applying a pressure of about 1.5 tons per square inch (22800.5 kPa) .8. Cn
机译:1.一种将平坦的预先形成的坯料转变成模制的模制门皮的方法,包括以下步骤:a)执行中密度纤维板的实心板; b)润湿毛坯并使其膨胀。 c)将加热的坯料置于板压机之间,将板加热至足以软化坯料中的树脂从而软化坯料的温度; d)施加足以夹持板和托的压力,从而使预成型件变形为由板的形状限定的成形形式; e)给坯件除气; f)从模制的二苯胺之间的轮廓空间中取出模制坯料。 2.根据权利要求1所述的方法,包括以下步骤:a)至少在三个tsiklov.3期间向所述板施加压力。 3.根据权利要求2所述的方法,包括以下步骤:a)向所述板施加不超过六个齐克洛夫的压力。4。 3.根据权利要求2所述的方法,包括以下步骤:a)在第一周期中将压力施加到第一预定水平,该时间段大于在随后的任何tsikle中施加压力的时间段。 3.根据权利要求2所述的方法,其特征在于,包括以下步骤:a)在最后一个循环中将压力保持一段时间,超过在第一tsikle中保持压力的时间段。 2.根据权利要求1所述的方法,其特征在于,所述方法包括通过在步骤7中的至少一个中的孔去除水分来进行工件脱气的操作。 7.根据权利要求6所述的方法,包括以下步骤:a)施加约1.5吨/平方英寸(22800.5kPa).8的压力。 n

著录项

  • 公开/公告号RU99123628A

    专利类型

  • 公开/公告日2005-02-27

    原文格式PDF

  • 申请/专利权人 МДФ ИНК (US);

    申请/专利号RU19990123628

  • 发明设计人 МОЙЕС ХАРТЛИ (GB);

    申请日1998-04-09

  • 分类号B27N3/10;E06B3/78;

  • 国家 RU

  • 入库时间 2022-08-21 22:01:44