摘要

A sulfurous compound such as a sulfur-rich "float" (concentrate) obtained by flotation of the residue from the leaching of a zinc concentrate is heated at a temperature not lower than the melting point of sulfur but below its boiling point, preferably not higher than 200 DEG C, more preferably not higher than 140 DEG C, and the evolving gas containing sulfur vapor is cooled at a temperature less than the melting point of sulfur, preferably at ordinary temperature, to condense sulfur. IMAGE
机译:在不低于硫的熔点但低于其沸点的温度下加热诸如硫的化合物,例如通过从锌精矿的浸出中浮选残渣而得到的富硫“浮选”(浓缩物)。在低于200℃,更优选不高于140℃的温度下,将含有硫蒸气的逸出气体在低于硫的熔点的温度下冷却,优选在常温下进行冷凝。 <图像>

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号