PROBLEM TO BE SOLVED: To provide a method for operating a blast furnace with which the ventilation in the furnace is improved by using sintered ore excellent in a high temperature reducibility and a large quantity of pulverized fine coals can be injected.;SOLUTION: In the method for operating the blast furnace, in which the injecting quantity of the pulverized fine coals is ≥150 kg/p-t, the sintered ore having 5-10 vol% porosity exceeding 50μm pore diameter and 5-15 vol% porosity at less than 5μm pore diameter in ≥70 mass% of iron oxide charging material charged from the furnace top, is used. As the above sintered ore, the sintered ore having 3.8-4.6 mass% content of SiO2 component and 5-9 mass% content of FeO component, is desirable to use and further, the sintered ore which is sintered by using a sintering raw material blended at 25-80 mass% high crystallization water ore having ≥4 mass% ratio of the crystallization water content, is desirable to use.;COPYRIGHT: (C)2006,JPO&NCIPI
机译:解决的问题:提供一种操作高炉的方法,通过使用高温还原性优异的烧结矿改善高炉的通风,并且可以注入大量的粉状细煤。一种操作高炉的方法,其中粉煤的喷射量为150kg / pt,烧结矿的孔隙率5-10%(体积)超过50μm,孔隙率5-15%(体积)。使用从炉顶部装入的氧化铁装入材料的小于或等于5μm的孔径(按质量计)的70质量%。作为上述烧结矿,期望使用具有SiO 2 成分的质量百分比为3.8〜4.6,FeO成分为5〜9质量%的烧结矿,此外,优选为通过使用以结晶水含量的比率为4质量%以上的25-80质量%的高结晶水矿石混合的烧结原料进行烧结是理想的。版权所有:(C)2006,JPO&NCIPI

著录项

  • 公开/公告号JP2006028538A

    专利类型

  • 公开/公告日2006-02-02

    原文格式PDF

  • 申请/专利权人 SUMITOMO METAL IND LTD;

    申请/专利号JP20040204943

  • 发明设计人 MATSUMURA MASARU;HOSHI MASAHIKO;

    申请日2004-07-12

  • 分类号C21B5/00;C22B1/16;

  • 国家 JP

  • 入库时间 2022-08-21 21:53:33

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号