Method for producing low nitrogen-containing chromium molten steel

机译:低含氮铬钢水的生产方法

摘要

PPROBLEM TO BE SOLVED: To provide a method for producing molten low nitrogen and chromium-containing steel by which molten low nitrogen and high purity chromium-containing steel is provided by reducing a degassing treatment in a reduced-pressure secondary decarburization-refining process and the shortening of a treating time in a reduced-pressure secondary decarburization-refining furnace, the reduction of a refractory cost, etc., can be obtained. PSOLUTION: A reduction-treatment of chromium oxide in slag is applied by dividedly adding COSB2/SBgenerating material 13 after adding a reduced agent into the molten chromium-containing steel performing the decarburization- refining in a converter 1. Successively, the reduced-pressure secondary decarburization-refining is applied after tapping off the chromium-containing steel 8 performing the reduction treatment in a ladle 12 charging the COSB2/SBgenerating material 13. PCOPYRIGHT: (C)2004,JPO
机译:

要解决的问题:提供一种用于生产熔融低氮和含铬钢的方法,通过该方法通过在减压二次脱碳精炼中减少脱气处理来提供熔融低氮和高纯含铬钢。可以实现减压二次脱碳精制炉中的处理工序的缩短,处理时间的缩短,耐材成本的降低等。

解决方案:渣中氧化铬的还原处理是在将还原剂添加到熔融的含铬钢中进行脱碳精炼后,分别添加CO 2 生成材料13进行的。转炉1。接着,在钢水包12中放出进行了还原处理的含铬钢8的放出后,进行减压二次脱碳精制。

版权:(C)2004,日本特许厅

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号