Method for producing sewage sludge incinerated ash solidified product

机译:污泥焚烧灰固化产物的生产方法

摘要

PROBLEM TO BE SOLVED: To decrease the amount and the volume of sewage sludge incineration ash, efficiently utilize the treated ash as a resource, provide a solid matter with high strength and scarcely eluting acids, heighten the plasticity of clay-like substance at the time of kneading, make it easy to adjust the curing speed, and improve the processibility at the time of a kneading work and a forming work. SOLUTION: Iron oxide or manganese dioxide is added to an incineration ash of sewage sludge generated by using a polymer flocculant, an acid-mixed solution produced by mixing an acid and water and keeping the mixture at room temperature or lower is further added to the incinerator ash mixture, the resultant mixture is kneaded while being kept at room temperature of lower, and the obtained clay-like substance is formed. Concretely, 9-15 cc of a 97% concentration sulfuric acid, 25-45 cc of water, and 1-3 g of iron oxide or manganese dioxide are added to 100 g of incinerator ash of sewage sludge generated by using a polymer flocculant and the resultant mixture is kneaded by an open type grinding and kneading apparatus.
机译:解决的问题:为减少污水污泥焚烧灰的数量和体积,有效利用处理后的灰作为资源,提供具有高强度和几乎不洗脱酸的固体物质,提高当时的粘土状物质的可塑性混炼时,容易调整固化速度,提高混炼时和成形时的加工性。解决方案:将氧化铁或二氧化锰添加到使用高分子絮凝剂产生的污泥的焚烧灰中,再将酸和水混合并保持在室温或更低温度下生成的酸混合溶液被添加到焚化炉中灰混合物,在保持较低的室温下捏合所得混合物,并形成获得的粘土状物质。具体而言,将9-15 cc浓度为97%的硫酸,25-45 cc的水和1-3 g的氧化铁或二氧化锰添加到100 g的使用聚合物絮凝剂产生的污水污泥的焚烧炉灰中。将所得混合物通过开放式研磨和捏合设备捏合。

著录项

  • 公开/公告号JP3746366B2

    专利类型

  • 公开/公告日2006-02-15

    原文格式PDF

  • 申请/专利权人 三機工業株式会社;

    申请/专利号JP19970353447

  • 发明设计人 前田 明徳;

    申请日1997-12-22

  • 分类号B09B3;C04B7/28;

  • 国家 JP

  • 入库时间 2022-08-21 21:49:26

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号