This invention relates to a method for the protection against corrosion of steel parts made of austenitic or semi-austenitic steel during the production of sulfuric acid. To improve the corrosion resistance of the steel parts which are in contact with the sulfuric acid, it is proposed to use austenitic or semi-austenitic steel which has a Cr content of 15 wt-% to 36 wt-% and an Ni content of 9 wt-% to 60 wt-% and in which the ratio of the chemical elements (Cr+Si)/(Ni+Mo) lies in the range from 0.9 to 1.9 or in which the ratio of the chemical elements Cr/(Ni+Mo) lies in the range from 0.8 to 1.5, and to additionally provide this steel part with an anodic corrosion protection.
机译:本发明涉及一种在硫酸生产过程中防止由奥氏体或半奥氏体钢制成的钢零件腐蚀的方法。为了改善与硫酸接触的钢部件的耐腐蚀性,提出使用Cr含量为15重量%至36重量%且Ni含量为9的奥氏体或半奥氏体钢。 wt-%至60 wt-%且其中化学元素(Cr + Si)/(Ni + Mo)的比率在0.9至1.9的范围内或其中化学元素Cr /(Ni + Mo)在0.8至1.5的范围内,并且另外为该钢部件提供阳极腐蚀保护。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号