FLUORESCENT MATERIAL, METHODE FOR SYNTHESIZING FLUORESCENT MATERIAL AND LIGHT EMITTING DIODE COATED WITH FLUORESCENT MATERIAL

机译:荧光材料,用于合成荧光材料的方法以及涂覆有荧光材料的发光二极管

摘要

The present invention, strontium carbonate (SrCO 3) and the flow path oxide europium (Eu 2 O 3) and is manufactured in a first step, the first step 1 of preparing a fluorescent mixture of orthosilicate group by mixing Methylsilsesquioxan (CH 3 SiO 1.5) a second step of preparing a phosphor by the primary heat treatment made for 1 to 10 hours fluorescent mixture in an oxidizing condition at a temperature of 900 ~ 1500 ℃, first of 1100 ~ 1500 ℃ in reducing the primary heat-treating the phosphor in the step 2, conditions a third step of the second heat treatment consisting for 1 to 10 hours at a temperature, in the first step 5 to release the particles with entangled during step 4, the fluorescent substance pulverized by a fourth step of pulverizing the secondary heat-treated phosphor in step 3 is configured, can be produced round the phosphor particles can reduce the variation in the size of the phosphor particles and provides a phosphor synthesis method that can adjust the size of the phosphor particles.
机译:本发明的碳酸锶(SrCO 3)和流路氧化物euro(Eu 2 O 3)是在第一步中制造的,第一步是通过混合甲基倍半硅氧烷(CH 3 SiO 1.5)制备正硅酸酯基团荧光混合物的第二步,第二步是通过对1〜10小时的荧光粉混合物在氧化条件下于900〜1500℃的温度下进行,首先在1100〜1500℃的温度下还原第一步骤中的荧光粉进行热处理,第二步骤的第三步骤为在温度下经过1到10个小时,在第一步5中释放出纠缠在步骤4中的颗粒,可以配置通过在步骤3中将第二次热处理的荧光粉粉碎的第四步来粉碎的荧光物质。磷光体颗粒可以减少磷光体颗粒尺寸的变化并提供磷phor合成法,可以调节荧光粉的粒径。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号