The present invention mixes a small amount of new materials such as cement, fly ash, lime and the like in the waste cement and fine powder obtained in the process of manufacturing recycled aggregates from recycled aggregates, such as waste concrete, by coating the surface of the recycled aggregates , Recycled waste cement and fines are easily recycled. Also, recycled aggregate coated with cement has excellent ionic bond with asphalt, so that it is possible to produce high quality asphalt concrete using recycled aggregate, waste cement and fine powder. The purpose of the present invention is to provide a cement-coated mixed aggregate using recycled aggregate and waste cement, and an asphalt concrete manufacturing method using the same.;Cement-coated mixed aggregate using recycled aggregate and waste cement according to the present invention for achieving the above object is a recycled coarse aggregate and recycled fine aggregate and crushed waste concrete at the same size; Mixed with the recycled coarse aggregate and the reclaimed coarse aggregate, and the waste cement and fine powder separated and extracted in the production process of the regenerated coarse aggregate and regenerated coarse aggregate; The recycled coarse aggregate and recycled fine aggregate and waste cement and fine particles are mixed with cement, fly ash, characterized in that consisting of a new material consisting of lime.;In addition, the asphalt concrete manufacturing method using a cement-coated mixed aggregate according to the present invention for achieving the above object is to crush the waste concrete to a suitable size over several times, such as by crushing the waste concrete, and after filtering the crushed residual particles to the screen, Washing with water or separating into a separation facility to produce recycled coarse aggregate and recycled fine aggregate; Preparing a cement-coated wet aggregate by mixing a small amount of new material with the waste cement and the fine powder obtained in the manufacturing process of the recycled coarse aggregate and the regenerated coarse aggregate into a mixer; Preparing a cement-coated mixed aggregate by curing the cement-coated wet aggregate for a predetermined time; The cement-coated mixed aggregate and a predetermined amount of asphalt is put into an asphalt plant, characterized in that the step of producing asphalt concrete by mixing.
机译:本发明将少量的新材料例如水泥,粉煤灰,石灰等混入废水泥和细粉中,这些废粉和细粉是通过从诸如废混凝土之类的再生集料制造再生集料的过程中获得的,其表面被涂覆。回收的骨料,回收的废水泥和细料易于回收。而且,涂有水泥的再生骨料与沥青具有优异的离子键,因此可以使用再生骨料,废水泥和细粉生产高质量的沥青混凝土。本发明的目的是提供一种使用再生骨料和废水泥的水泥包覆的混合骨料,以及使用其的沥青混凝土的制造方法。实现上述目的的是相同尺寸的再生粗骨料,再生细骨料和压碎废混凝土。与再生的粗骨料和再生的粗骨料混合,在再生的粗骨料和再生的粗骨料的生产过程中将废水泥和细粉分离并提取;将再生的粗骨料和再生的细骨料以及废水泥和细颗粒与水泥,粉煤灰混合,其特征在于,其由石灰组成的新材料组成;此外,使用水泥涂层的混合骨料制造沥青混凝土的方法根据本发明的用于实现上述目的的方法是将废混凝土粉碎多次至合适的尺寸,例如通过粉碎废混凝土,并且在将粉碎的残余颗粒过滤到筛网上之后,用水洗涤或分离成小颗粒。分离设施,以生产回收的粗骨料和回收的细骨料;通过将少量的新材料与废水泥和在回收的粗骨料和再生的粗骨料的制造过程中获得的细粉混合,制备水泥包覆的湿骨料;通过将水泥涂覆的湿集料固化预定时间来制备水泥涂覆的混合集料;将涂有水泥的混合骨料和预定量的沥青放入沥青厂,其特征在于,通过混合来生产沥青混凝土的步骤。

著录项

  • 公开/公告号KR20050115358A

    专利类型

  • 公开/公告日2005-12-07

    原文格式PDF

  • 申请/专利权人 MIN WON;

    申请/专利号KR20040040174

  • 发明设计人 MIN WON;

    申请日2004-06-03

  • 分类号C04B18/16;

  • 国家 KR

  • 入库时间 2022-08-21 21:27:54

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号