REPAIR METHOD FOR INNERFACE OF AN OVERAGE VESSEL

机译:多余容器内部的修复方法

摘要

The present invention occurs when a specific part and weld corrosion on the inside of the antiquated various pressure reservoir, corrosion by allowing the epoxy resin is a full two inner drive storage container with the non-woven fabric impregnated with the reservoir primarily padded inner surface by coating with an epoxy resin is an epoxy resin-coated waterproof layer is formed to surround the generation region enough rice, various according to a long-term use of the pressure storage vessel that can effectively prevent corrosion occurs in part on its inner surface to extend the service life of the various pressure storage container, the storage container in a state where the contents stored therein completely discharged removal of rust removing rust formed on the inner surface area of the rust step (S1) and; Forcibly forced drying process (S2) and dried by using a blowing against corrosion region of the storage container is removed rust; The dried epoxy resin is forced against corrosion by bonding a non-woven fabric impregnated with the first portion bonded nonwoven fabric so that the waterproof layer is a step of forming (S3) and; Nature such that the corrosion area is an epoxy resin-impregnated non-woven fabric bonded to the inner surface coated with an epoxy resin storage vessel for the entire second waterproof layer so as to form a resin coating step of (S4) and an epoxy resin is applied to air-dry the inner surface of the storage vessel the drying step (S5) the compensation method the inner surface of the old pressure reservoir characterized in that a.
机译:当过时的各种压力储存器的内部发生特定部位的焊接腐蚀时,本发明就发生了,该腐蚀是通过使环氧树脂为一个完整的两个内部驱动存储容器,其中无纺布浸渍有储存器,从而主要填充了内部表面。用环氧树脂涂覆的是形成环氧树脂涂层的防水层,以围绕生米区足够的大米,根据长期使用的储压容器的不同,可以有效地防止部分腐蚀发生在其内表面上以扩大各种压力存储容器的使用寿命,其中存储容器中的内容物完全排出了在除锈步骤(S1)的内表面上形成的除锈除锈的状态,并且;强制进行干燥工序(S2),并用吹干的方法对贮藏容器的腐蚀部位进行除锈处理;通过使浸渍有第一部分粘合无纺布的无纺布粘合,从而使干燥的环氧树脂耐腐蚀,从而使防水层成为形成工序(S3)。腐蚀区域是在整个第二防水层上粘结有涂有环氧树脂存储容器的内表面的环氧树脂浸渍无纺布的性质,从而形成了(S4)的树脂涂覆步骤和环氧树脂适用于风干存储容器的内表面,干燥步骤(S5),补偿方法是旧压力容器的内表面,其特征在于:a。

著录项

  • 公开/公告号KR20060000191A

    专利类型

  • 公开/公告日2006-01-06

    原文格式PDF

  • 申请/专利权人 YOON SANG KUK;

    申请/专利号KR20040048746

  • 发明设计人 YOON SANG KUK;

    申请日2004-06-28

  • 分类号F17B1/00;B65D90/00;

  • 国家 KR

  • 入库时间 2022-08-21 21:27:00

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号