invention the barium calcium titanate (BaCaTiO 3 ) of the powder preparation and It relates to a multilayer ceramic capacitor using the same . This manufacturing method , BaTiO 3 BaTiO powder to the slurry containing the 3 for the 100 moles of mixing a water-soluble salt of Ca and 0.5 to 2.5 mol , spray- drying the slurry next , heat treatment at a temperature of 800 ~ 1200 to BaCaTiO 3 to obtain a powder is also provided a multilayer ceramic capacitor using the powder .