The invention waste concrete, conventional water-permeable concrete paving through the recycling of fly ash and silica fume water permeability and strength characteristics compared to, ability and durability that provide excellent security, a method for producing a high-performance water-permeable polymer concrete driveway paving, ordinary Portland cement or blast furnace slag cement, grain size of 5 ~ 8mm, 5 ~ 13mm of Crushed and lungs concrete recycled aggregate, 5-20 wt% of the mass ratio of the acrylic polymer or rubber polymer with respect to the use of cement, silica fume as an admixture with 5 to 30 parts by weight each with respect to the fly ash used binder%, 0 to 30% by weight, use, and bending 0.2 to 2.0 parts by weight of steel fibers or polypropylene fibers for reinforcement to secure the toughness and crack resistance to the binder%, high-performance AE water-reducing agent or a superplasticizer 0.5 for improving fluidity in the binder mass ratio compared to 3.0 wt% incorporated by design porosity 8 to 25%, the water-binder ratio is prepared by in the 20 ~ 30%
机译:本发明通过回收粉煤灰和硅粉而废弃的常规的透水性混凝土铺路,与水相比,透水性和强度特性,提供优异安全性的能力和耐久性,一种高性能透水性聚合物混凝土车道的生产方法摊铺,普通硅酸盐水泥或高炉矿渣水泥,粒度为5〜8mm,5〜13mm的碎屑和肺部混凝土再生骨料,相对于用途而言,丙烯酸聚合物或橡胶聚合物的质量比为5-20 wt%水泥,硅粉的混合物,分别相对于所用粉煤灰为5至30重量份,0至30重量%,使用,并弯曲0.2至2.0重量份的钢纤维或聚丙烯纤维增强粘合剂的韧性和抗裂性的粘合剂,高性能AE减水剂或高效减水剂0.5用于改善粘合剂质量比中的流动性,而incor为3.0 wt%由设计孔隙率定为8%至25%,水结合剂比例为20%至30%

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号