首页> 外国专利> SULFOALUMINOUS CLINKER HAVING A HIGH BELITE CONTENT, PROCESS FOR PRODUCING SUCH A CLINKER AND USE THEREOF FOR PREPARING HYDRAULIC BINDERS.

SULFOALUMINOUS CLINKER HAVING A HIGH BELITE CONTENT, PROCESS FOR PRODUCING SUCH A CLINKER AND USE THEREOF FOR PREPARING HYDRAULIC BINDERS.

机译:具有高贝氏体含量的硫磺粉煤灰,生产这种粉煤灰的过程,并将其用于制备液压粘合剂。

摘要

The invention relates to a belite-sulphoaluminous clinker, to its manufacturing process and its use for the preparation of hydraulic binders, and comprising as mineralogical composition: 5 to 25%, preferably 10 to 20%, of calcium aluminoferrite phase; a composition corresponding to the general formula C2AXF (1-X), with X between 0.2 and 0.8 - 15 to 35%, preferably 20 to 30%, of calcium sulfoaluminate phase "yee 'limit" (C4A3 $), - 40 to 75%, preferably 45 to 65% belite (C2S), - from 0.01 to 10% of one or more minor phases chosen from calcium sulphates, alkaline sulphates, perovskite, aluminates calcium, gehlenite, free lime and periclase, and / or a glassy phase, and at least one secondary element selected from sulfur, magnesium, sodium, potassium, boron, phosphorus, zinc, manganese, titanium, fluorine, chlorine, the total content of the said secondary elements ires being less than or equal to 15%.
机译:本发明涉及一种珍珠岩-硫铝熟料,涉及其制造方法及其在制备水硬性粘结剂中的用途,并包含作为矿物学组合物的5-25%,优选10-20%的铝铁氧体钙相。对应于通式C2AXF(1-X)的组合物,其中X为0.2至0.8-15%至35%,优选20%至30%的硫铝酸钙相“ yee'limit”(C4A3 $),-40至75 %,优选45%至65%的珍珠岩(C2S),-0.01%至10%的一种或多种次要相,选自硫酸钙,碱式硫酸盐,钙钛矿,铝酸钙,钠钙石,游离石灰和钙镁石和/或玻璃态以及选自硫,镁,钠,钾,硼,磷,锌,锰,钛,氟,氯中的至少一种次级元素,所述次级元素的总含量小于或等于15%。

著录项

  • 公开/公告号FR2873366A1

    专利类型

  • 公开/公告日2006-01-27

    原文格式PDF

  • 申请/专利权人 LAFARGE;

    申请/专利号FR20040051586

  • 发明设计人 ELLIS GARTNER;GUANSHU LI;

    申请日2004-07-20

  • 分类号C04B28/06;C04B7/32;

  • 国家 FR

  • 入库时间 2022-08-21 21:17:22