The invention relates to a belite-sulphoaluminous clinker, to its method of manufacture and its use for the preparation of hydraulic binders, and comprising as a mineralogical composition: 5 to 25%, preferentially 10 to 20% of calcium aluminoferrite phase of a composition corresponding to the general formula C2AXF (1-X), with X ranging from 0.2 to 0.8. - 15 to 35%, preferentially 20 to 30%, calcium sulphoaluminate phase 'yee' limit (C4A3 $), - 40 to 75%, preferably 45 to 65% belite (C2S), - from 0.01 to 10% of one or more minor phases selected from calcium sulphates, alkaline sulfates, perovskite, calcium aluminates, gehlenite, free lime and periclase, and / or a glassy phase, and at least one secondary element selected from sulfur, magnesium, sodium, potassium, boron, phosphorus, zinc, manganese, titanium, fluorine, chlorine, the total content of said secondary elements being lower or equal to 15%.
机译:本发明涉及一种贝利特-硫铝熟料,其制造方法及其在制备水硬性粘结剂中的用途,并且包含作为矿物学组合物的:组成的5-25%,优选10-20%的钙铝铁氧体相。通式C2AXF(1-X),X的范围为0.2到0.8。 -硫铝酸钙相'yee'限值(C4A3 $)的15%至35%,优选20%至30%,-珍珠岩(C2S)的40%至75%,优选45%至65%,-一种或多种的0.01%至10%选自硫酸钙,碱式硫酸盐,钙钛矿,铝酸钙,钠钙石,游离石灰和钙镁石的次要相,和/或玻璃态相,以及选自硫,镁,钠,钾,硼,磷,锌的至少一种次级元素,锰,钛,氟,氯,所述次级元素的总含量低于或等于15%。

著录项

  • 公开/公告号CA2574532C

    专利类型

  • 公开/公告日2012-11-06

    原文格式PDF

  • 申请/专利权人 LAFARGE;

    申请/专利号CA20052574532

  • 发明设计人 GARTNER ELLIS;LI GUANSHU;

    申请日2005-07-19

  • 分类号C04B7/32;C04B28/06;

  • 国家 CA

  • 入库时间 2022-08-21 17:20:43

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号