Interlaminar tensile reinforcement of SiC/SiC CMC's using fugitive fibers

机译:短纤维对SiC / SiC CMC的层间拉伸增强

摘要

A method of manufacturing a turbine engine component is disclosed. The method includes the steps of providing a plurality of ceramic cloth plies, each ply having woven ceramic fiber tows and at least one fugitive fiber tow, laying up the plurality of plies in a preselected arrangement to form a turbine engine component shape, oxidizing the fugitive fibers to produce fugitive fiber void regions in the ply, rigidizing the component shape to form a coated component preform using chemical vapor infiltration, partially densifying the coated component preform using carbon-containing slurry, and further densifying the coated component preform with at least silicon to form a ceramic matrix composite turbine engine component having matrix rich regions.
机译:公开了一种制造涡轮发动机部件的方法。该方法包括以下步骤:提供多个陶瓷布层片,每个层片具有编织的陶瓷纤维丝束和至少一个短纤维丝束,以预选的布置方式放置多个层片以形成涡轮发动机部件的形状,将短丝氧化物氧化纤维以在层中产生逃逸的纤维空隙区域,使用化学气相渗透来硬化部件形状以形成涂覆的部件预成型件,使用含碳的浆料部分地使涂覆的部件预成型件致密化,并进一步用至少硅致密化涂覆的部件预成型件至形成具有基质富集区域的陶瓷基质复合涡轮发动机组件。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号