An activated carbon that is capable of adsorbing taste-and-odor-causing and other organic compounds, wherein the activated carbon comprises a uniquely modified carbonaceous material. The activated carbon comprising: (a) a pore volume per gram of the activated carbon more than about 0.32 mL in the pore width range between about 4 to 63 angstroms; and (b) a pore volume per gram of the activated carbon more than about 0.21 mL in the pore width range between about 63 to 500 angstroms; provided that the pore volume per gram of the activated carbon in the pore width range of about 20 to 63 angstroms is at least about 25% of the total pore volume per gram of the activated carbon in the pore width range of 4 to 63 angstroms, as measured per the Argon Adsorption Density Functional Theory protocol; provided that the activated carbon has a pH equal to or greater than 9.9, when immersed as a slurry in nitrogen-purged deionized distilled water, while the slurry contains about 10% by weight of activated carbon, as measured per the Slurry pH protocol.
机译:能够吸收引起味道和气味的有机化合物和其他有机化合物的活性炭,其中所述活性炭包括独特改性的碳质材料。活性炭包括:(a)每克活性炭的孔体积在约4至63埃之间的孔宽范围内大于约0.32mL; (b)在约63至500埃的孔宽度范围内,每克活性炭的孔体积大于约0.21mL;只要在约20至63埃的孔宽度范围内每克活性炭的孔体积为在约4至63埃的孔宽度内每克活性炭的总孔体积的至少约25%,根据氩吸附密度泛函理论协议进行测量;前提条件是,当将活性碳以浆液形式浸入氮气吹扫的去离子蒸馏水中时,其活性炭的pH值等于或大于9.9,而根据浆液pH方案测得,该浆液中约含10%重量的活性炭。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号