A method of forming a composite structure comprises: (1) providing a first and a second sintered bodies comprising a first and a second multicomponent metallic oxides having similar a first and a second crystal structures, which are a perovskite and a fluorite; (2) providing a joint material comprising at least one metal oxide, which (a) comprises (i) at least one metal of an identical Group of the IUPAC periodic table as at least one sintered body metal in one of the first multicomponent metallic oxide, (ii) a first row D-Block transition metal not contained in the first multicomponent metallic oxides and/or (iii) a lanthanide not contained in the first multicomponent metallic oxides; (b) is free of metals contained in the first multicomponent metallic oxides; (c) is free of cations of boron, silicon, germanium, tin, lead, arsenic, antimony, phosphorous, and tellurium; and (d) has a melting point below the sintering temperatures of said sintered bodies; and (3) heating the sintered bodies and the joint material to a joining temperature above the melting point and below the sintering temperatures.
机译:一种形成复合结构的方法,包括:(1)提供第一和第二烧结体,所述第一和第二烧结体包括钙钛矿和萤石的具有相似的第一和第二晶体结构的第一和第二多组分金属氧化物; (2)提供一种包含至少一种金属氧化物的接头材料,其中(a)包括(i)至少一种与第一多组分金属氧化物之一中的至少一种烧结体金属相同的IUPAC周期表族的至少一种金属。 (ii)第一多组分金属氧化物中不包含的第一行D-Block过渡金属和/或(iii)第一多组分金属氧化物中不包含的镧系元素; (b)不含第一多组分金属氧化物中所含的金属; (c)不含硼,硅,锗,锡,铅,砷,锑,锑,磷和碲的阳离子; (d)熔点低于所述烧结体的烧结温度; (3)将烧结体和接合材料加热至熔点以上且低于烧结温度的接合温度。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号