A method of increasing the length of life of heating elements that consist essentially of molybdenum-silicide, and alloys thereof, when the elements are operated at a low temperature, such as at a temperature ranging from 400-600° C. The heating element material contains Mo(SiSUB1-x/SUBAlSUBx/SUB)SUB2/SUB, and that material contains sufficient aluminum to substantially prevent the formation of pest.
展开▼
机译:当加热元件在低温下,例如在400-600℃范围内的温度下工作时,增加基本上由硅化钼及其合金组成的加热元件的寿命的方法。加热元件材料含有Mo(Si 1-x SUB> Al x SUB>) 2 SUB>,该材料含有足够的铝以基本上防止有害生物的形成。
展开▼