A noble metal hydrocracking catalyst which has high selectivity for naphtharange products and a process for its preparation areprovided. The hydrocracking catalyst comprises: (a) from 70 to 95 weightpercent of a Y zeolite, based on the catalyst having a silica toalumina mole ratio of from 4.8 to less than 6.0, a unit cell constant in therange of 24.50 to 24.57, an Na2O level of less than or equalto 0.25 weight percent; (b) from 10 to 30 weight percent, based on thecatalyst: of an alumina having a mercury intrusion pore volume inthe range from 0.55 to 0.85 cc/g; and (c) from 0.5 to 1 weight percent, basedon the catalyst of a noble metal; wherein said hydrocrackingcatalyst has a dispersivity of the noble metal of equal or greater than 48 %by hydrogen chemisorption measurement, a surface area ofgreater than or equal to 690 m2/g by BET surface area measurement, a compactedbulk density in the range of from 0.40 to 0.58 g/cc, anda mercury pore volume in the range of from 0.4 to 0.7 ml/g.
机译:对石脑油具有高选择性的贵金属加氢裂化催化剂系列产品及其制备过程是提供。加氢裂化催化剂包含:(a)70至95重量%的Y沸石,基于具有二氧化硅的催化剂氧化铝的摩尔比为4.8至小于6.0,在Na 2 O水平小于或等于24.50至24.57至0.25重量%; (b)10至30重量百分比,基于催化剂:一种具有汞侵入孔体积的氧化铝0.55至0.85 cc / g的范围; (c)0.5至1重量百分比,基于在贵金属的催化剂上;其中所述加氢裂化催化剂对贵金属的分散度等于或大于48%通过氢化学吸附测量,表面积为通过BET表面积测量得出大于或等于690 m2 / g的压实堆积密度在0.40至0.58 g / cc的范围内,并且汞孔体积在0.4至0.7 ml / g的范围内。

著录项

  • 公开/公告号CA2283283C

    专利类型

  • 公开/公告日2007-10-30

    原文格式PDF

  • 申请/专利权人 SHELL CANADA LIMITED;

    申请/专利号CA19982283283

  • 申请日1998-03-19

  • 分类号B01J29/12;B01J37/08;B01J37/30;C10G47/18;

  • 国家 CA

  • 入库时间 2022-08-21 20:54:12

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号