摘要

Group IV nanocrystals, such as, for example, silicon nanocrysals and germanium nanocrystals, with chemically accessible surfaces are produced in solution reactions. Group IV halides can be reduced in organic solvents such as 1,2-dimethoxyethane (glyme), with soluable reducing agents to give halide-terminated group IV nanocrystals, which can then be easily functionalized with alkyl lithium, Grignard or other reagents to synthesize group IV nanocrystals having air and moisture stable surfaces. Synthesis can occur at ambient temperature and pressure.
机译:在溶液反应中产生具有化学可及表面的IV族纳米晶体,例如硅纳米晶体和锗纳米晶体。 IV类卤化物可在有机溶剂(例如1,2-二甲氧基乙烷(甘醇二甲酸酯)中)与可溶性还原剂还原,生成卤化物封端的IV类纳米晶体,然后可以轻松地用烷基锂,格氏试剂或其他试剂官能化以合成具有空气和水分稳定表面的IV纳米晶体。合成可以在环境温度和压力下进行。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号