首页> 外国专利> Method for producing metal oxide nanorods, metal oxide nanorods and composite material containing these nanorods thus obtained

Method for producing metal oxide nanorods, metal oxide nanorods and composite material containing these nanorods thus obtained

机译:由此获得的金属氧化物纳米棒的制造方法,金属氧化物纳米棒和包含这些纳米棒的复合材料

摘要

Methods of preparing metal oxide nanorods are described. The metal oxide nanorods have diameters between 1 and 200 nm and aspect ratios between 5 and 2000. The methods include the steps of generating a metal vapor in a furnace, exposing the nanorod growth substrate to the metal vapor within a growth zone in the furnace for a sufficient time to grow metal oxide nanorods on a surface of the nanorod growth substrate, removing the nanorod growth substrate from the growth zone after the sufficient time to grow metal oxide nanorods on a surface of the nanorod growth substrate, and removing the metal oxide nanorods from the furnace. The methods can be used to prepared large quantities of metal oxide nanorods.
机译:描述了制备金属氧化物纳米棒的方法。金属氧化物纳米棒的直径在1至200nm之间,长径比在5至2000之间。该方法包括以下步骤:在炉中产生金属蒸气,将纳米棒生长衬底暴露于炉中的生长区域内的金属蒸气中,以进行加热。足够的时间在纳米棒生长基板的表面上生长金属氧化物纳米棒,在足够的时间在纳米棒生长基板的表面上生长金属氧化物纳米棒之后,从生长区中移除纳米棒生长基板,并去除金属氧化物纳米棒从熔炉。该方法可用于制备大量的金属氧化物纳米棒。

著录项

  • 公开/公告号EP0885316B1

    专利类型

  • 公开/公告日2006-11-15

    原文格式PDF

  • 申请/专利权人 HARVARD COLLEGE;

    申请/专利号EP19970907700

  • 发明设计人 YANG PEIDONG;LIEBER CHARLES M.;

    申请日1997-02-21

  • 分类号C30B23/00;C30B29/16;C30B29/60;B32B5/02;H01L39/02;

  • 国家 EP

  • 入库时间 2022-08-21 20:51:28