Waste rubber in the from of crumbs, mainly from automobile tires, but also from other used rubber products including waste rubber formed in the course of their manufacturing, is mixed in a kneader, calender, or extruder with a compound containing the chemical group -SO2-NH-. Subsequently, at temperatures up to 180 °C the rubber crumbs are de-vulcanized within 15-20 minutes, the de-vulcanization degree being controlled by the de-vulcanization agent concentration, and time and temperature of de-vulcanization. After the eventual addition of small amounts of extenders as oil, soot, raw rubber, inorganic filler and the vulcanization agent a vulcanization mixture is obtained that after pressing into the shape of the rubber product is subjected to a standard vulcanization process.
机译:将来自面包屑的废橡胶(主要来自汽车轮胎,也来自其他用过的橡胶产品,包括在其制造过程中形成的废橡胶)在捏合机,压延机或挤出机中与包含化学基团-SO2的化合物混合-NH-随后,在高达180°C的温度下,橡胶屑在15-20分钟内脱硫,脱硫程度由脱硫剂浓度,脱硫时间和温度控制。在最终加入少量增量剂如油,烟灰,生橡胶,无机填料和硫化剂后,得到硫化混合物,其在压制成橡胶制品的形状后进行标准的硫化过程。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号