A method for improving the heat stability of a film of poly-p-xylylene or a derivative thereof as represented by the general formula (1), which comprises forming a film through chemical deposition from a raw material prepared by mixing a (2.2) -paracyclophane represented by the general formula (2) with an amino-(2.2) -paracyclophane represented by the general formula (3) and by which the heat resistance of the film can be improved without impairing the deposition properties or the economic efficiency; and poly-p-xylylene derivatives improved in heat resistance: (1) [wherein X1 and X2 are each hydrogen, lower alkyl, or halogeno, and they may be the same or different from each other; and n is a degree of polymerization], (2) [wherein X1 and X2 are each the same as defined for the general formula (1)], and (3) [wherein X3 is hydrogen or lower alkyl; and Y1 and Y2 are each hydrogen or amino, with the proviso that both of Y1 and Y2 must be not hydrogen]. ® KIPO & WIPO 2007
机译:一种改善通式(1)表示的聚对亚二甲苯基或其衍生物的膜的热稳定性的方法,该方法包括通过化学沉积由混合(2.2)的原料制备的原料形成膜。通式(2)表示的对环环烷与通式(3)表示的氨基-(2.2)-对环环烷,可以在不损害沉积性或经济性的情况下提高膜的耐热性。 (1)[式中,X 1和X 2分别为氢,低级烷基或卤代基,可以相同也可以不同。 n为聚合度],(2)[其中X1和X2分别与通式(1)所定义的相同]]和(3)[其中X3为氢或低级烷基; [式中,Y 1和Y 2分别为氢或氨基,条件是Y 1和Y 2都必须不是氢]。 ®KIPO和WIPO 2007

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号