Provided are a cement inorganic grouting material composition which is gel type, is environmentally friendly and has a high strength, and a method for grouting the composition for boring grouting work. The cement inorganic grouting material composition comprises: a first composition which comprises 85-99 wt% of a common CSA-based cement having a fineness of 6,000-9,000 cm^2/g, and 1-15 wt% of at least one kind of accelerator selected from the group consisting of chlorides, carbonates, sulfates, acetates, silicates and hydroxides containing a metal ion of potassium, sodium, calcium and aluminum; and a second composition which comprises 50-90 wt% of a Portland cement having a fineness of 3,000-9,000 cm^2/g, 10-50 wt% of anhydrous gypsum or hemihydrate gypsum, 1-10 wt% of at least one accelerator selected from carbonates and hydroxides of a metal ion of lithium and calcium, 0-30 wt% of kiln dust, and 0.5-2.0 wt% of at least one kind of dispersant selected from naphthalene sulfonate, melamine sulfonate and polycarbonate.
机译:提供了一种凝胶型,环保且具有高强度的水泥无机灌浆材料组合物,以及一种将该组合物灌浆以进行钻孔灌浆工作的方法。该水泥无机灌浆材料组合物包括:第一组合物,其包含85-99 wt%的细度为6,000-9,000 cm ^ 2 / g的普通CSA基水泥和1-15 wt%的至少一种促进剂,其选自包含钾,钠,钙和铝的金属离子的氯化物,碳酸盐,硫酸盐,乙酸盐,硅酸盐和氢氧化物;第二种组合物,其包含50-90重量%的细度为3,000-9,000cm 2 / g的波特兰水泥,10-50重量%的无水石膏或半水石膏,1-10重量%的至少一种促进剂。选自锂和钙的金属离子的碳酸盐和氢氧化物,0-30重量%的窑灰和0.5-2.0重量%的选自萘磺酸盐,三聚氰胺磺酸盐和聚碳酸酯中的至少一种分散剂。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号