The present invention relates to a manufacturing method for improving the ridging property of ferritic stainless steel containing 16-20% chromium (Cr). In the present invention, by weight%, C 0.05% or less, Ti 0.7% or less, Si 1.0% or less, Mn 1.0% or less, P 0.04% or less, S 0.03% or less, Cr 16.0-20%, Ni 0.5% or less, Mo 1.0 When hot rolling a stainless steel slab composed of% or less, N 0.05% or less, Cu 1.0% or less, Al 0.15% or less, balance Fe and other common impurities, the rolling reduction step is 40% or more. The ferritic stainless steel having excellent leasing characteristics, characterized in that at least three passes having a reduction ratio of 30% or more in finishing rolling, and four or more passes having a shape factor (l / d) value of 3.5 or more. It provides a manufacturing method.;Ferrite, Stainless, Leasing, Rolling Rate, Shape Factor
机译:本发明涉及一种用于改善含16-20%铬(Cr)的铁素体不锈钢的起皱性能的制造方法。在本发明中,以重量%计,C为0.05%以下,Ti为0.7%以下,Si为1.0%以下,Mn为1.0%以下,P为0.04%以下,S为0.03%以下,Cr为16.0〜20%。 ,Ni 0.5%以下,Mo 1.0热轧由以下%,N 0.05%以下,Cu 1.0%以下,Al 0.15%以下,余量的Fe和其他常见杂质构成的不锈钢板时,轧制率降低。步长为40%或更高。具有优异的租赁特性的铁素体不锈钢,其特征在于,精轧中至少有3道次的压下率为30%以上,并且有至少4道次的形状系数(l / d)值为3.5以上。它提供了一种制造方法。;铁素体,不锈钢,租赁,轧制率,形状系数

著录项

  • 公开/公告号KR100706529B1

    专利类型

  • 公开/公告日2007-04-12

    原文格式PDF

  • 申请/专利权人 POSCO;

    申请/专利号KR20050129406

  • 申请日2005-12-26

  • 分类号C21D8;C22C38;

  • 国家 KR

  • 入库时间 2022-08-21 20:32:29

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号