首页> 外国专利> METHOD OF MANUFACTURING BUILDING INSIDE FINISH MATERIAL USING NEGATIVE ION MATERIAL AND CONSTRUCTING WITH THAT MATERIAL

METHOD OF MANUFACTURING BUILDING INSIDE FINISH MATERIAL USING NEGATIVE ION MATERIAL AND CONSTRUCTING WITH THAT MATERIAL

机译:用负离子材料制造建筑物内部材料并用该材料构造的方法

摘要

The present invention relates to a method of manufacturing an interior finishing material using an anion material and a construction method using the finishing material. More specifically, an anion material (powder) manufactured by using a blast furnace slag is mixed in cement or a building finishing material. To prevent the occurrence of bleaching and mold bacteria caused by cement, concrete, etc., or by applying a spray coating on building materials or wallpaper in buildings to prevent the occurrence of mold bacteria. It relates to a construction method using the finishing material.;The present invention is to prepare a second mixture by mixing a mixture of cement and blast furnace slag in an anionic material (powder) at a ratio of 8: 2, and 20-40% by weight of sand, lime, etc. And a step of adding 60-70% by weight of water to the second mixture to form a liquid liquid dough with fluidity, and further comprising a finishing material using an anion material manufactured by this method. The surface of the plaster, concrete, and brick is completely dried to less than 1 to 2% by weight, and then the finish of the liquid dough is applied by applying an air compressor or the like with a thickness of 0.2 mm to 0.3 mm. It features.;Anion material, finishing material, powder, liquid, whitening, mold, construction
机译:本发明涉及一种使用阴离子材料制造内部装饰材料的方法以及一种使用该装饰材料的建筑方法。更具体地,将通过使用高炉矿渣制造的阴离子材料(粉末)混合在水泥或建筑装饰材料中。为了防止由水泥,混凝土等引起的漂白和霉菌的发生,或在建筑物的建筑材料或墙纸上喷涂涂料以防止霉菌的发生。本发明涉及通过将水泥和高炉矿渣的混合物与阴离子材料(粉末)以8:2和20-40的比例混合来制备第二混合物的方法。以及向第二混合物中添加60-70%重量的水以形成具有流动性的液态面团的步骤,该步骤还包括使用通过该方法制造的阴离子材料制成的整理材料。将石膏,混凝土和砖块的表面完全干燥至小于1至2重量%,然后通过使用厚度为0.2 mm至0.3 mm的空气压缩机等对液体面团进行精加工。 。它具有以下特点:阴离子材料,表面处理材料,粉末,液体,增白,发霉,结构

著录项

  • 公开/公告号KR100762505B1

    专利类型

  • 公开/公告日2007-10-04

    原文格式PDF

  • 申请/专利权人

    申请/专利号KR20050087417

  • 申请日2005-09-20

  • 分类号C04B18/14;C04B28;

  • 国家 KR