A method of carrying out ECAP(Equal Channel Angular Process) of magnesium materials is provided to conduct an ECAP(equal channel angular process) of magnesium materials even at room temperature. A method of carrying out ECAP(Equal Channel Angular Process) of a magnesium material at room temperature comprises the following steps of: preheating the magnesium material to a temperature of 300 to 340 deg.C; extruding the preheated magnesium material; heat-treating the extruded magnesium material at 350 to 450 deg.C; and performing the ECAP of the heat-treated magnesium material at the room temperature. The magnesium material is extruded at an extrusion ratio of 15:1 to 30:1. The heat treatment process is conducted in an atmosphere of an inert gas such as argon, helium or nitrogen for 20 to 28 hours. The ECAP process is performed at an intersection angle of 120 to 150 degrees at which two channels intersect with each other. The ECAP process is performed at 45 to 60 degrees of a curvature angle of channels. The ECAP process is performed one to four times.
机译:提供了一种进行镁材料的ECAP(等通道角过程)的方法以即使在室温下也进行镁材料的ECAP(等通道角过程)。一种在室温下进行镁材料的ECAP(等通道角加工)的方法,包括以下步骤:将镁材料预热至300至340℃的温度;挤出预热的镁材料;在350至450℃下对挤出的镁材料进行热处理。并在室温下对热处理后的镁材料进行ECAP。镁材料以15:1至30:1的挤出比被挤出。热处理过程在惰性气体如氩气,氦气或氮气中进行20至28小时。以两个通道彼此相交的120到150度的相交角执行ECAP处理。在通道的曲率角为45至60度时执行ECAP处理。 ECAP过程执行一到四次。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号