PROBLEM TO BE SOLVED: To provide a manganese dry cell having a negative electrode zinc can superior in corrosion resistance.;SOLUTION: Added elements other than zinc are precipitated in crystal grain boundary of zinc to constitute the negative electrode zinc can 4. The added elements are made of at least one kind of element selected from Pb, Bi, Ca, Mg, Si, Al, In. Furthermore, the zinc can 4 is formed by cooling molten zinc containing added elements at a cooling speed of 75-100°C/sec to diecast a zinc plate and the cast zinc plate is formed in the can by impact molding at a temperature of 20-30°C.;COPYRIGHT: (C)2008,JPO&INPIT
机译:解决的问题:提供一种具有负极锌罐的锰干电池,该锌罐的耐腐蚀性优异。;解决方案:除锌以外的添加元素沉淀在锌的晶界中以构成负极锌罐4。添加的元素它们是由选自Pb,Bi,Ca,Mg,Si,Al,In中的至少一种元素制成的。此外,通过以75-100℃/秒的冷却速度冷却包含添加元素的熔融锌以压铸锌板来形成锌罐4,并且通过在20℃的温度下进行冲模来在罐中形成铸锌板。 -30°C;版权:(C)2008,JPO&INPIT

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号