摘要

PROBLEM TO BE SOLVED: To provide a high-strength and high thermal expansion austenitic stainless steel excellent in high-temperature settling resistance and corrosion resistance, and to provide its manufacturing method.;SOLUTION: This high-strength and high thermal expansion austenitic stainless steel has a composition consisting of 0.10-0.30 wt.% C, ≤ 3.0 wt.% Si, ≤ 3.0wt.% Mn, 5.0-12.0 wt.% Ni, 18.0-30.0 wt.% Cr, and 0.05-0.30 wt.% N, and the balance Fe with inevitable impurities. The area ratio of carbide and carbo-nitride precipitated in a metal structure of the stainless steel is below 3%, and the Ni equivalent expressed by expression 1, ( Ni equivalent = 24.2C + 13.7N + 0.35Si + 0.5Mn + Ni + 0.65Cr) is 24.0-30.0 wt.%.;COPYRIGHT: (C)2004,JPO
机译:要解决的问题:提供一种具有优异的耐高温沉降性和耐腐蚀性的高强度高热膨胀性奥氏体不锈钢,并提供其制造方法。具有由0.10-0.30重量%的C组成的成分, 3.0重量%的Si,≤ Mn为3.0重量%,Ni为5.0-12.0重量%,Cr为18.0-30.0重量%,N为0.05-0.30重量%,余量的Fe具有不可避免的杂质。在不锈钢的金属结构中析出的碳化物和碳氮化物的面积比低于3%,用表达式1表示的Ni当量(Ni当量= 24.2C + 13.7N + 0.35Si + 0.5Mn + Ni + 0.65Cr)为24.0-30.0 wt。%.;版权:(C)2004,JPO

著录项

  • 公开/公告号JP4034129B2

    专利类型

  • 公开/公告日2008-01-16

    原文格式PDF

  • 申请/专利权人 日本冶金工業株式会社;

    申请/专利号JP20020175298

  • 发明设计人 鈴木 治;池上 雄二;

    申请日2002-06-17

  • 分类号C22C38/00;B21B1/22;B21B3/02;C21D9/46;C22C38/58;

  • 国家 JP

  • 入库时间 2022-08-21 20:18:31

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号