PROBLEM TO BE SOLVED: To obtain an agglomerate having scarcely reductively powdering and good reducibility by pre-reducing hematite ore to change magnetite powdery ore and agglomerating the powdery ore.;SOLUTION: The pre-reducing temp. of the hematite ore is desirable to 750°C. Further, when the magnetite powdery ore is agglomerated, carbon is desirable to contain. Concretely, the carbon is beforehand contained in the hematite ore and when the magnetite powdery ore is agglomerated, the carbon quantity may be increased. The obtd. agglomerate is not made to reduced powdering and has good high temp. property and good reducibility. Because in the case of executing the pre-reduction at 750°C, many fine pores are formed and the total porosity becomes high. Further, the magnetite powdery ore is agglomerated into small grains having 3-10 mm grain diameter and the agglomerate combining plural grains has the best reducibility. That is, the smaller the single grain for agglomerate is, the higher the reducibility of the agglomerate is.;COPYRIGHT: (C)2000,JPO
机译:解决的问题:通过预还原赤铁矿矿石以改变磁铁矿粉状矿石和使粉状矿石结块,获得具有几乎不还原性粉化和良好还原性的附聚物;解决方案:预还原温度。 <750℃的赤铁矿矿石是理想的。此外,当将磁铁矿粉矿附聚时,期望包含碳。具体地,碳预先包含在赤铁矿矿石中,并且当磁铁矿粉状矿石附聚时,碳量可以增加。奥特。附聚物不能减少粉化并且具有良好的高温。性能和良好的还原性。因为在<750℃下进行预还原的情况下,形成许多细孔并且总孔隙率变高。此外,将磁铁矿粉矿团聚成具有3-10mm粒径的小颗粒,并且将多个颗粒结合的团块具有最佳还原性。也就是说,团聚体的单颗粒越小,团聚体的还原性就越高。;版权:(C)2000,JPO

著录项

  • 公开/公告号JP4149080B2

    专利类型

  • 公开/公告日2008-09-10

    原文格式PDF

  • 申请/专利权人 新日本製鐵株式会社;

    申请/专利号JP19990148939

  • 发明设计人 内藤 誠章;

    申请日1999-05-27

  • 分类号C21B5/00;

  • 国家 JP

  • 入库时间 2022-08-21 20:18:07

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号