Ammonium sulphate nitrate is produced in a multistage reaction system which comprises a mixing stage and a granulation stage, followed by a cooling stage, the parameters in both stages are adjusted in such a way that ammonium nitrate undergoes maximum reaction to double salt, ammonium nitrate sulphate suspension is prepared in a continuous process in a mixing unit by feeding ammonium nitrate melt, dolomite and ammonium sulphate into the reactor, the contents of the reactor is thoroughly mixed, with continuous heat input supplied to maintain a preferable temperature for the process of 120°C (not lower), the time the reaction mixture should remain in the reactor should not exceed the total time of the granulation stage and the drying stage, ammonium nitrate sulphate pulp is subsequently directed to a multistage granulation system, preferably a two-stage system, consisting of a 2 shaft granulator equipped with a moisturizing system (the first granulation step) and a drum granulator (the second granulation step), the time the mixture remains in the second stage granulator is at least twice shorter than the time of the mixing stage, preferably about 8-10 times shorter, the final product of proper granularity is dried, screened, cooled, bagged and shipped.
机译:硫酸铵是在一个多阶段反应系统中生产的,该系统包括一个混合阶段和一个制粒阶段,然后是一个冷却阶段,调节两个阶段的参数,使硝酸铵最大程度地反应成双盐硫酸铵。通过将硝酸铵熔体,白云石和硫酸铵进料到反应器中,在混合装置中以连续过程制备悬浮液,将反应器中的物料充分混合,并提供连续的热量输入,以保持过程中120°C的最佳温度C(不低于),反应混合物应保留在反应器中的时间不应超过制粒阶段和干燥阶段的总时间,随后将硝酸铵硫酸盐浆引导至多阶段制粒系统,优选为两阶段系统由两轴造粒机(带保湿系统)(第一步制粒)和转鼓造粒机(s在第2阶段制粒机中),混合物保留在第二阶段制粒机中的时间至少比混合阶段的时间短两倍,优选短约8-10倍,将适当粒度的最终产品干燥,过筛,冷却,装袋并发货。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号