The invention relates to the field of ferrous metallurgy. A method of charging of electric arc furnace for melting of titaniferous raw material involves two stage loading of mixture of titaniferous ores and hard carbonaceous materials in multiple parts in the peripheral areas of the furnace and in the central area of the furnace between electrodes, at that on the first stage 18-25 % of charge is loaded through the central charging pipe, at that mass of charge, which is loaded is of 1.2-1.7 t per 1 MVA of supplied power, and on the second stage charge is loaded evenly through the central and peripheral charging pipes in a quantity of 4.5-5.5 t per 1 MVA of supplied power, at that the total quantity of the loaded charge through central charging pipe is of 37-47 %. In addition, quantity of the carbon reducing agent which is contained in carbonaceous materials, in the charge of the first and second load is of 70-80 % from a necessity on melting, and the other reducing agent is additionally introduced after melting of charge in the pure form. The invention allows to increase efficiency of melting process of titaniferous material.
机译:本发明涉及黑色冶金领域。一种用于熔化钛铁原料的电弧炉的装料方法包括在炉子的周边区域和电极之间的炉子中心区域的多个部分中分两阶段加载钛铁矿和硬碳材料的混合物。在第一阶段,通过中央充电管加载18-25%的电荷,按该电荷质量计,每1 MVA供电功率为1.2-1.7 t,在第二阶段,电荷均匀地通过中心和外围充电管的数量为每1 MVA供电4.5-5.5 t,通过中心充电管的装料总量为37-47%。另外,从熔融的需要出发,第一负荷和第二负荷的进料中的碳质材料中所含的碳还原剂的量为70〜80%,另外,在进料熔融后,另外导入其他的还原剂。纯形式。本发明允许增加钛质材料的熔化过程的效率。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号