This invention provides a tape-like oxide superconducting wire rod comprising a plurality of filaments containing a Bi-2223-type oxide superconductor embedded in a matrix. The sectional area in a cross section perpendicular to the longitudinal direction of the oxide superconducting wire rod is not more than 0.5 mm2. In the cross section of the oxide superconducting wire rod, the average sectional area per filament can be brought to not less than 0.2% and not more than 6% of the sectional area of the oxide superconducting wire rod to enhance the critical current density and, at the same time, to lower the alternating-current loss. There are also provided a superconducting structure, a method of manufacturing the oxide superconducting wire rod, a superconducting cable, a superconducting magnet, and a product comprising the superconducting magnet.
机译:本发明提供了一种带状氧化物超导线材,其包括多个细丝,所述细丝包含嵌入基质中的Bi-2223型氧化物超导体。垂直于氧化物超导线材的长度方向的截面中的截面积为0.5mm 2以下。在氧化物超导线材的横截面中,每根灯丝的平均截面积可以不小于氧化物超导线材的截面积的0.2%且不大于6%,以提高临界电流密度,并且,同时,降低交流损耗。还提供了一种超导结构,一种氧化物超导线材的制造方法,一种超导电缆,一种超导磁体,以及一种包括该超导磁体的产品。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号