An amorphous microwire coated with an insulating sleeve, consisting of a metal core made up of an alloy of transition metals and metalloid elements, at a proportion between 65%-90% and 10%-35%, respectively, and an insulating glass sleeve; the transition metals are at least iron, the relative proportion of iron being between 65%-100% of the total transition metals, and the core diameter (Dc) is comprised between 2 µm and 20 µm,such that the magnetostriction constant (λ) of the metal alloy is comprised between 1 and 30 ppm, and the natural ferromagnetic resonance frequency is comprised between 3 and 20 GHz.;The invention also refers to a method for the manufacture of an amorphous microwire.
机译:一种无定形微线,其上涂有绝缘套,由绝缘玻璃套和绝缘玻璃套组成,绝缘套由过渡金属和准金属元素的合金组成,金属核的比例分别为65%-90%和10%-35%。过渡金属至少为铁,铁的相对比例为过渡金属总量的65%-100%,芯直径(D c )在2 µm至20 µm之间,因此,金属合金的磁致伸缩常数(λ)在1至30ppm之间,并且自然铁磁共振频率在3至20GHz之间。本发明还涉及用于制造非晶微线的方法。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号