FIELD: technological processes.;SUBSTANCE: method involves ingot casting by electroslag refining; turning and drilling of central hole in ingots; ingot heating to the elasticity temperature; piercing at piercing mill to form shells; shell rolling at pilger mill to form conversion pipes of 290x12x23000-24000 mm dimensions. Rolling of front ends at (1.0-1.2) Lrec length is performed for Sf=Sy+K wall width, and rolling of rear ends at (1.2-1.5) Lrec length is performed for Sr=Sy-K1 wall width, where Lrec=1100-1150 is recoil distance of feeder during rolling 290 mm diameter pipes in rolls with 980 mm barrel diameter, mm; Sf is front end pipe wall thickness, mm; Sy=12 is rated wall thickness of conversed pipes for regular rolling process, mm; Sr is rear end pipe wall thickness, mm; K=(2-3) is growth factor of pipe wall thickness during front end rolling, mm; Kl=(0.5-0.8) is diminishment factor of pipe wall thickness during rear end rolling, mm.;EFFECT: reduced metal expenditure and cost of commercial hexagon pipes.;1 tbl
机译:领域:工艺流程;实质:该方法涉及通过电渣精炼铸造铸锭;铸锭中心孔的车削和钻孔;铸锭加热至弹性温度;在冲孔机上冲孔以形成壳;在pilger轧机上进行壳层轧制,以形成290x12x23000-24000 mm尺寸的转换管。对于S f = S y + K壁宽,以(1.0-1.2)L rec 长度滚动前端,然后滚动对S r = S y -K 1 进行(1.2-1.5)L rec 长度的后端壁宽,其中L rec = 1100-1150是进料器在290毫米直径的管子在直径980毫米的辊子中轧制时进给的反冲距离; S f 是前端管道壁厚,mm; S y = 12是常规轧制对接管的额定壁厚,mm; S r 是后端管的壁厚,mm; K =(2-3)是前端轧制时管壁厚度的增长因子,mm; K l =(0.5-0.8)是后端轧制过程中管壁厚度的减小因子,mm。效果:减少了金属成本,降低了商用六角管的成本。1tbl

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号