A capacitor comprising an aluminum anode and a dielectric layer comprising phosphate doped aluminum oxide and process for making the capacitor. The capacitor has a CV Product of at least 9 μF−V/cm2 at 250 volts. Furthermore, the capacitor is formed by the process of: forming an aluminum plate; contacting the plate with an anodizing solution comprising glycerine, 0.1 to 1.0%, by weight, water and 0.01 to 0.5%, by weight, orthophosphate; applying a voltage to the aluminum plate and determining an initial current; maintaining the first voltage until a first measured current is no more than 50% of the initial current; increasing the voltage and redetermining the initial current; maintaining the increased voltage until a second measured current is no more than 50% of the redetermined initial current, and continuing the increasing of the voltage and maintaining the increased voltage until a final voltage is achieved.
机译:一种包括铝阳极和包括磷酸盐掺杂的氧化铝的介电层的电容器及其制造方法。该电容器在250伏特时的CV积至少为9μF-V/ cm 2 。此外,通过以下步骤形成电容器:使所述板与包含0.1-1.0重量%的甘油和0.01-0.5重量%的正磷酸盐的阳极氧化溶液接触;向铝板施加电压并确定初始电流;保持第一电压直到第一测量电流不超过初始电流的50%;增加电压并重新确定初始电流;保持增加的电压,直到第二个测得的电流不超过重新确定的初始电流的50%为止,并继续增加电压并保持增加的电压,直到达到最终电压为止。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号