Polymer compositions exhibiting enhanced flow-induced crystallization

机译:聚合物组合物表现出增强的流动诱导结晶

摘要

Provided is a polymer composition having a linear, semi-crystalline thermoplastic matrix polymer and a second thermoplastic polymer. The second polymer is a substantially saturated hydrocarbon polymer including (i) a backbone chain and (ii) one or more substantially hydrocarbon sidechains connected to the backbone chain. The sidechains each have a number-average molecular weight of from 2,500 g/mol to 125,000 g/mol and an MWD by SEC of 1.0 to 3.5. The mass ratio of sidechain molecular mass to backbone molecular mass is from 0.01:1 to 100:1. The matrix polymer is present at 95 wt % or more based on the weight of the composition. The second polymer is present at 0.2 to 5.0 wt % or more based on the weight of the composition. Provided is also a method for enhancing flow-induced crystallization in a linear, semi-crystalline thermoplastic matrix polymer. Provided is also a method for processing a polymer composition.
机译:提供了具有线性,半结晶的热塑性基质聚合物和第二热塑性聚合物的聚合物组合物。第二聚合物是基本饱和的烃聚合物,其包括(i)主链和(ii)一个或多个连接至主链的基本烃侧链。每个侧链的数均分子量为2,500g / mol至125,000g / mol,通过SEC的MWD为1.0至3.5。侧链分子量与主链分子量的质量比为0.01∶1至100∶1。基于组合物的重量,基质聚合物的存在量为95重量%以上。基于组合物的重量,第二聚合物的存在量为0.2至5.0重量%或更高。还提供了一种用于增强线性,半结晶热塑性基体聚合物中的流致结晶的方法。还提供了用于加工聚合物组合物的方法。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号