首页> 外国专利> Atmospheric Pressure Leach process for Nickel ore LATERu00cdTICO

Atmospheric Pressure Leach process for Nickel ore LATERu00cdTICO

机译:镍矿石的大气压浸提工艺

摘要

An atmospheric leaching process in the Recovery of nickel and Cobalt from laterite ores, the process includes the steps of: (a) to separate the Ore lateru00edtico in a fraction of a Mineral containing Magnesium,And a fraction of ore containing High Magnesium through Selective Post Mining or mining Classification; (b) separately from the slurry separated fractions of Mineral leaching; (c) The fraction of Mineral containing Magnesium with Concentrated sulfuric acid as a At the primary stage of leaching; and (d) introduce the mineral slurry containing High Magnesium to continBirth through twenty-one continu of substantial completion of the primary stage of leaching and precipitation of Iron as goethite or other form of iron oxide or hydroxide of Iron containing sulfate, sulfuric acid released during the precipitation of Iron, is used for the l The fraction of ixiviaciu00f3n ore with high Magnesium as a secondary leaching stage.
机译:从红土矿石中回收镍和钴的一种常压浸出工艺,该工艺包括以下步骤:(a)将矿石中的矿石分离成一部分含镁矿物和一部分含高镁矿石通过选择性后期采矿或采矿分类; (b)与泥浆分离的矿物浸出部分分开; (c)浸出初级阶段含镁的矿物质与浓硫酸的比例; (d)连续二十一个基本完成铁的浸出和沉淀的初级阶段的连续过程,使含高镁的矿物泥浆继续生矿,铁为针铁矿或其他形式的铁氧化物或含铁的氢氧化物,其中硫酸盐,硫酸在铁的沉淀用于第二阶段浸出的高镁ixiviaci u00f3n矿石的馏分。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号