Selective Leaching Nickel from the Pre-reduced Limonitic Laterite Ore at Atmospheric Pressure

机译:选择性浸出镍从预先降低的唇原矿石处处于大气压

获取原文

摘要

In this paper a novel method for selective leaching nickel from pre-reduced laterite ore at atmospheric pressure was reported. The reduced calcine was leached in thin acid liquor to liberate the nickel and iron together firstly. By properly controlling the leaching condition, the leached iron ion could hydrolyze as goethite precipitate and regenerate the acid consumed in the leaching procedure. Finally, the nickel is selectively extracted into the leaching solution. The main factors in the leaching process, such as reduction degree of the laterite ore, acidity of the leaching solution were investigated as influence on the nickel extraction. The test results showed that selectively leaching of nickel could be achieved with an extraction degree up to 90% by reducing most of the iron in the lateritic ore to wuestite and controlling the pH value of the leaching solution below 2.5.
机译:本文报道了一种新的方法,用于在大气压下从预减薄的后卫矿石中选择性浸出镍。将还原煅烧在薄的酸性液中浸出,首先将镍和铁释放。通过适当地控制浸出条件,浸出的铁离子可以水解,因为聚氨酸沉淀物,并再生浸出过程中消耗的酸。最后,选择性地将镍选择为浸出溶液。浸出过程中的主要因素,例如红土矿石的还原程度,浸出溶液的酸度作为对镍提取的影响。试验结果表明,通过将外层矿石中的大部分铁减少到威氏菌素并控制低于2.5以下的浸出溶液的pH值,可以通过提取程度浸出镍的选择性浸出。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号