PROCEDURE FOR THE QUICK REALIZATION OF PROTOTIPOS BY SINTERED LASER POWDER.

机译:烧结激光粉快速实现原形的方法。

摘要

Procedure for rapid prototyping, by means of a laser, a powder or a mixture of powders, especially ceramics, comprising the steps consisting of: 1 / obtaining a succession of numbered superimposed sections (10) of an object (12 ) which is intended to make, from a three-dimensional representation of said object, 2 / spread in the form of a thin layer (14) the powder or the mixture of powders heated to a temperature close to the sintering temperature of said powder or of said mixture of powders, 3 / heating at the sintering temperature by sweeping with a laser beam (16) a selected part (18) of the layer, corresponding to one of the numbered sections (10 '') of the object (12) that is to be carried out, repeating steps 2 and 3 until obtaining all the numbered superimposed sections of the object to be performed, characterized in that the selected part (18) of the layer is sintered in solid phase merc ie to the supplementary contribution of energy of the laser and because the density of the powder or the powder mixture of the layer (14) is previously increased with respect to sintering.
机译:借助激光,粉末或粉末混合物(尤其是陶瓷)进行快速原型制作的程序,包括以下步骤:1 /获得物体(12)的连续编号的重叠部分(10)的序列,旨在从所述物体的三维表示中,以薄层(14)的形式制成粉末/粉末混合物,将其加热至接近所述粉末或粉末混合物的烧结温度的温度。 ,3 /通过用激光束(16)扫掠该层的选定部分(18)以在烧结温度下进行加热,该层对应于将要携带的物体(12)的编号部分(10'')之一然后,重复步骤2和3,直到获得要执行的对象的所有编号的重叠部分,其特征在于,层的选定部分(18)以固相烧结,即对激光的能量和能量的补充贡献。因为密度相对于烧结,层(14)的粉末或粉末混合物事先被增加。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号