An atmospheric leaching process for the recovery of a nickel and cobalt from a lateritic ore includes (a) preparing a slurry of the lateritic ore with saline or hypersaline water having a total dissolved solids (TDS) content greater than 30 g/L; (b) leaching the slurry of the lateritic ore with sulfuric acid at atmospheric pressure, and (c) recovering nickel and cobalt from the resultant leachate.
展开▼
机译:从红土矿石中回收镍和钴的常压浸出工艺包括:(a)用总溶解固体含量大于30 g / L的盐水或高盐度水制备红土矿石的浆液; (b)在大气压下用硫酸浸提红土矿石的浆液,和(c)从所得浸出液中回收镍和钴。
展开▼