首页> 外国专利> Process For Atmospheric Leaching Of Laterite Ores Using Hypersaline Leach Solution

Process For Atmospheric Leaching Of Laterite Ores Using Hypersaline Leach Solution

机译:高盐浸出液对红土矿石进行大气浸出的方法

摘要

An atmospheric leaching process for the recovery of a nickel and cobalt from a lateritic ore, said process including the steps: (a) preparing a slurry of the lateritic ore with saline or hypersaline water having a total dissolved solids (TDS) content greater than 30 g/L; (b) leaching the slurry of the lateritic ore with sulfuric acid at atmospheric pressure, (c) recovering nickel and cobalt from the resultant leachate.
机译:一种用于从红土矿石中回收镍和钴的大气浸出方法,所述方法包括以下步骤:(a)用总溶解固体(TDS)含量大于30的盐水或高盐度水制备红土矿石的浆液克/升(b)在大气压下用硫酸浸提红土矿石的浆液,(c)从所得浸出液中回收镍和钴。

著录项

  • 公开/公告号US2011056333A1

    专利类型

  • 公开/公告日2011-03-10

    原文格式PDF

  • 申请/专利权人 HOUYUAN LIU;GRAHAM ANDREW REYNOLDS;

    申请/专利号US20090920546

  • 发明设计人 HOUYUAN LIU;GRAHAM ANDREW REYNOLDS;

    申请日2009-03-19

  • 分类号C22B23;C01G53/11;C01G53/04;C01G53/06;C01G51/04;C01G51/06;C01G51;

  • 国家 US

  • 入库时间 2022-08-21 18:11:15

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号