A kind of method offer of the hydrophobic PTFE coating on the carbon steel heating element for being coated with enamel for GGH, wherein a good bumps is occurred in enamel coating layer. A kind of method of the hydrophobic PTFE coating on the carbon steel heating element for being coated with enamel for GGH is comprising steps of do the surface of the slightly enamel coating layer in first with blasting treatment, in order to increase the adhesivity of fluorine resin coating and enamel coating layer; Formed by spray with about 3-4mum thickness hydrophobic fluorine resin coating or immersing liquid a step, wherein as polytetrafluoroethylene fluorine resin component on the enamel coating layer being etched by containing therefore be sintered it is blocking it. Under 150 and 350 degrees Celsius of temperature, the liquid that wherein fluorine resin is contained is sprayed on enamel coating layer and is sintered blocking 5 minutes~24 hours.
机译:提供了一种在碳钢加热元件上涂覆疏水性PTFE涂层的方法,以用于GGH搪瓷,其中在搪瓷涂层中出现了良好的凸点。在碳钢加热元件上涂覆GGH搪瓷的疏水性PTFE涂层的一种方法包括以下步骤:首先对第一微搪瓷涂层的表面进行喷砂处理,以增加氟树脂的附着力。涂层和搪瓷涂层;通过喷涂约3-4μm厚的疏水性氟树脂涂层或浸入液体而形成的步骤,其中,由于搪瓷涂层上的聚四氟乙烯氟树脂组分因被包含而被蚀刻而被烧结,因此将其阻塞。在150和350摄氏度的温度下,将包含氟树脂的液体喷涂到搪瓷涂层上,并烧结5分钟〜24小时。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号