A lead-free glass for forming barrier ribs is provided to be free of Li2O or contain less than 0.5% of Li2O and be suitable for use in forming barrier ribs of a plasma display panel. A lead-free glass for forming barrier ribs comprises, in terms of % by mass of the following oxides, 20-35% of B2O3, 25-60% of ZnO, 0-6% of SiO2, 0.1-10% of Al2O3, 3-38% of MgO+CaO+SrO+BaO, 0-0.3% of Li2O, and 0.1-6% of Na2O+K2O. The lead-free glass has a softening point of 600 ‹C or less, and an average linear thermal expansion coefficient of 60Î10^(-7) - 85Î10^(-7)/‹C at 50-350 ‹C. A glass ceramics composition for forming barrier ribs includes 100 parts by mass of a powder of the lead-free glass and 0.1-40 parts by mass of an inorganic oxide powder.
机译:提供用于形成障壁的无铅玻璃,该无铅玻璃不含Li 2 O或包含小于0.5%的Li 2 O,并且适合用于形成等离子显示面板的障壁。用于形成隔壁的无铅玻璃,按以下氧化物的质量百分比计,包括20-35%的B 2 O 3,25-60%的ZnO,0-6%的SiO 2,0.1-10%的Al 2 O 3, MgO + CaO + SrO + BaO的3-38%,Li2O的0-0.3%和Na2O + K2O的0.1-6%。无铅玻璃的软化点为600°C或更低,在50-350°C下的平均线性热膨胀系数为60°10 ^(-7)-85°10 ^(-7)/ ‹C。用于形成障壁的玻璃陶瓷组合物包括100质量份的无铅玻璃粉末和0.1-40质量份的无机氧化物粉末。

著录项

  • 公开/公告号KR100882769B1

    专利类型

  • 公开/公告日2009-02-09

    原文格式PDF

  • 申请/专利权人

    申请/专利号KR20070084467

  • 申请日2007-08-22

  • 分类号C03C3/062;C03C3/064;C03C3/066;C03C3/068;

  • 国家 KR

  • 入库时间 2022-08-21 19:12:11

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号