METHOD OF LOW-DEFORMING DIFFUSION WELDING OF ELEMENTS MADE FROM SINTERED NON-OXIDE CERAMICS AND WORKPIECE MADE FROM NON-OXIDE CERAMICS WITH SEAMLESS JOINT

机译:烧结非氧化物陶瓷元件的低变形扩散焊接和无缝接头非氧化物陶瓷制成的工件的方法

摘要

FIELD: welding jobs.;SUBSTANCE: invention can be used for jointing ceramic elements made from sintered non-oxide ceramics. The elements are brought in contact and jointed by diffusion welding in a low-deforming way, in the presence of protective gas and with a forced applied to form a monolith. Welding temperature makes at least 1600°C, preferably, over 1800°C, most desirable, over 2000°C. The method makes the elements to be jointed subjected to plastic strain less that 5%, and preferably less than 1%.;EFFECT: producing seamless monolith with shape complying with that of finished workpiece that allows rejecting subsequent mechanical processing.;19 cl, 7 dwg, 6 ex
机译:技术领域:本发明可用于接合由烧结的非氧化物陶瓷制成的陶瓷元件。在存在保护气体的情况下,通过扩散焊接以低变形的方式使元件接触并接合,并施加压力以形成整体。焊接温度至少为1600℃,优选超过1800℃,最希望超过2000℃。该方法使要连接的元件承受的塑性应变小于5%,最好小于1%。效果:生产形状与成品工件形状一致的无缝整料,从而可以拒绝后续的机械加工; 19 cl,7 dwg,6前

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号