PROBLEM TO BE SOLVED: To provide a technique for reuse waste tires produced in great volume around the world as a concrete pavement road surface paving material.;SOLUTION: Waste tire rubber chips 2 and 3 beaten into a length of 0.1 to 50 mm or cut into a size of 0.01 to 2,500 square millimeter are used as aggregates in the concrete pavement road paving material 1 wherein the aggregate of 10 pts.wt. is mixed with concrete of 10 to 500 pts.wt. Aggregates 6 made by pulverizing the waste tire into rubber chips of 0.1 to 5 mm of 10 pts.wt. is mixed with mortar of 10 to 500 pts.wt., so as to obtain a concrete pavement joint member 7 for filling into a joint for the concrete pavement as a dry molded board. Or the aggregates 6 made by pulverizing the waste tire into the rubber chips of 0.1 to 5 mm of 10 pts.wt. is mixed with mortar of 10 to 500 pts.wt., so as to obtain a concrete pavement joint member 9 for filling into the joint of the concrete pavement by a wet construction method.;COPYRIGHT: (C)2010,JPO&INPIT
机译:要解决的问题:提供一种技术来重复使用世界各地大量生产的废轮胎,作为混凝土路面铺路材料。解决方案:废轮胎橡胶碎片2和3被打成0.1至50毫米的长度或切成小块在混凝土路面铺路材料1中,骨料的厚度为0.01-2,500平方毫米的骨料被用作骨料,其中骨料为10pts.wt。与10至500 pts.wt的混凝土混合。通过将废轮胎粉碎成0.1到5毫米10磅重量的橡胶碎片制成的骨料6。将其与10至500pts.wt。的灰浆混合,从而获得混凝土路面接合构件7,其作为干模制板填充到用于混凝土路面的接合物中。或通过将废轮胎粉碎成0.1ptmm至5mm的10pts.wt的橡胶碎片制成的骨料6。将其与10至500 pts.wt.的灰浆混合,以获得通过湿法施工方法填充到混凝土路面缝中的混凝土路面缝构件9。版权所有:(C)2010,JPO&INPIT

著录项

  • 公开/公告号JP2010156187A

    专利类型

  • 公开/公告日2010-07-15

    原文格式PDF

  • 申请/专利权人 HOTTA NAOYOSHI;

    申请/专利号JP20090092650

  • 发明设计人 HOTTA NAOYOSHI;

    申请日2009-04-07

  • 分类号E01C7/10;

  • 国家 JP

  • 入库时间 2022-08-21 19:05:47

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号