PROBLEM TO BE SOLVED: To provide a low yield ratio, high strength and high toughness steel sheet producible with high production efficiency at low cost without increasing the stock cost by the addition of large quantities of alloy elements or the like and without deteriorating weld heat affected zone toughness, and to provide its production method.;SOLUTION: The low yield ratio, high strength and high toughness steel sheet comprises, by mass, 0.03 to 0.1% C, 0.01 to 0.5% Si, 1.2 to 2.5% Mn and ≤0.08% Al, and comprises at least two or more metals selected from 0.005 to 0.04% Ti, 0.005 to 0.07% Nb and 0.005 to 0.1% V, and the balance substantially Fe. In the steel sheet, C/(Ti+Nb+V) as a ratio between the C content and the total content of Ti, Nb and V by atomic% is 1.2 to 3, the metallic structure is substantially composed of the three phases of ferrite, bainite and insular martensite, and the area fraction of the insular martensite is 3 to 20%.;COPYRIGHT: (C)2005,JPO&NCIPI
机译:要解决的问题:提供一种低成本,高生产效率的低屈服比,高强度和高韧性钢板,而无需通过添加大量合金元素等来增加库存成本,并且不会降低焊接热影响解决方案:低屈服比,高强度和高韧性钢板按质量计包含0.03%至0.1%的C,0.01%至0.5%的Si,1.2%至2.5%的Mn和≤。 Al为0.08%,并且包含至少两种或多种选自0.005至0.04%的Ti,0.005至0.07%的Nb和0.005至0.1%的V的金属,其余基本上为Fe。在钢板中,C /(Ti + Nb + V)作为C含量与Ti,Nb和V的总含量之比以原子%计为1.2至3,金属组织基本上由以下三个相组成:铁素体,贝氏体和岛状马氏体,且岛状马氏体的面积分数为3%至20%。;版权所有:(C)2005,JPO&NCIPI

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号